NSN 9650-00-278-1522 · NIIN 002781522 · FSC 9650
NO DASHES 9650002781522
In Stock
INGOT,LEAD ALLOY
Nonferrous Base Metal Refinery and Intermediate Forms
Technical characteristics
4 rows
Straight from the federal item record. Entries the record leaves empty are shown empty — nothing is filled in on its behalf.
| MRC | Requirement | Value |
|---|---|---|
| BBRF | IMPURITIES LIMITATION IN PERCENT | ALUMINUM 0.005 MAX AND ANTIMONY 8.00 MIN TO 10.00 MAX AND ARSENIC 0.20 MAX AND COPPER 0.50 MAX AND IRON 0.10 MAX AND TIN 4.00 MIN TO 6.00 MAX AND ZINC 0.005 MAX AND OTHER ELEMENTS 0.75 MAX |
| ZZZT | NONDEFINITIVE SPEC/STD DATA | GRADE 13 |
| BBRC | COMPOSITION AND PERCENTAGE | MINIMUM BY VOLUME LEAD 83.00 AND MAXIMUM BY VOLUME LEAD 88.00 |
| AZQK | WEIGHT | POUNDS NOMINAL 10.0 |